Numéro |
J. Phys. I France
Volume 5, Numéro 5, May 1995
|
|
---|---|---|
Page(s) | 547 - 554 | |
DOI | https://doi.org/10.1051/jp1:1995150 |
J. Phys. I France 5 (1995) 547-554
From Quasi-Static to Rapid Fracture
E. Bouchaud and S. NavéosO.N.E.R.A. (OM), 29 Avenue de la Division Leclerc, B.P. 72, 92322 Châtillon Cedex, France
(Received 7 February 1995, accepted 24 February 1995)
Abstract
Four fracture profiles corresponding to four different crack velocities are studied on the same
sample and show the existence of a crossover lengthscale
decreasing with the crack velocity.
For lengthscales larger than
, the previously reported roughness index
is
recovered. At lengthscales smaller than
, the fracture profile fits with a quasi-static (QS)
hypothesis, i.e., the measured roughness index is close to
.
Résumé
Quatre profils de rupture correspondant à quatre vitesses de propagation de fissure différentes
sont étudiés sur le même échantillon, et révèlent l'existence d'une longueur de coupure
qui décroît avec la vitesse. Pour des échelles de longueur supérieures à
, on
retrouve un exposant de rugosité voisin de
. A plus petite échelle, l'exposant
mesuré est en accord avec une hypothèse de propagation quasi-statique (QS) du front de fissure,
et vaut
.
© Les Editions de Physique 1995